Almost all problems in the paint on the surface preparation is the result of insufficient or incorrect. Is not properly prepared surface to surface and hold the paint or paint the floor with the remaining dirt, oil or moisture shortly after paint layer leads to bloat up. Below the surface preparation is done indoors in case some of you will find problems that may arise.
/ Swell /
This problem is usually trapped between the paint and ground moisture is optional. The most important point to be aware that the surface is damp. Paint the bottom of your paint to come out of the remaining moisture surging Do not forget.
/ Soy, and fall /
Various surfaces and peeling occurs is directly related to the humidity. To know how to prepare different surfaces the best possible protection against this problem allows.
/ Wrinkle /
This problem is not usually pay attention to the normal dry period, the second layer is applied too early or is made in paint out very humid environment. Also very hot or very cold air when the paint or glossy surfaces without sanding is also observed wrinkle.
/ Fringe on the bottom of Soy /
Do not see the sun, peeling in places corresponding to the lower canopy is seen more often. Reason is still inadequate surface preparation. Environment caused by salt air and sun has been cleaned of paint, the problem again is inevitable.
/ Galvanized metal is in the Soy/
Occurs as a result of the surface can not hold paint. Reason for choosing the wrong primer or undercoat is not hit. Rust, oil and other substances to the surface of the painting and hold paint to be cleared before the blocks. Galvanized surface, then painted a very short time it is clear that the problem can be seen peeling.